MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® LR 3842/40 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Low oil-bleeding liquid silicone rubbers of the ELASTOSIL® LR 3842 series are paste-like, readily pigmentable two-component products with short curing times. Shortly after the curing process, a slight thin oil film with lubricating properties forms on the surface of the vulcanizates. The vulcanizates are opaque, have good mechanical and electrical properties and very low compression sets.

Properties: The products can be used within a temperature range of - 55 °C to + 210 °C. The addition of heat stabilizers at service temperatures of more than 180 °C is recommended.

Application: ELASTOSIL® LR 3842/40 A/B is particularly suitable for the economical production of weather packs in the automotive industry. They are increasingly being used to produce cable and connector seals. As an oil film forms, seals can be fitted easily and fully automatically, even when tolerances are narrow.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183-1 A
Viscosity 1.30e+6 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 38DIN 53505
Tensile Strength at Break 8.00 MPaDIN 53504 S 1
Elongation at Break 650 %DIN 53504 S 1
Tear Strength 25.0 kN/mASTM 624 B
Compression Set 14 %
@Temperature 175 °C,
Time 79200 sec
post cure, 1h/200°C; DIN ISO 815-B
 16 %
@Temperature 175 °C,
Time 79200 sec
DIN ISO 815-B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °Cwith heat stabilizer
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
in press
 
Descriptive Properties
Appearanceopaque
Fluid content (%)2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3003/40 A/B Liquid Silicone Rubber
Seals Eastern 5803 Fluoro-silicone
Wacker Elastosil® FLR 3900/40 A/B Liquid Fluorosilicone Rubber
Wacker Elastosil® FLR 3905/60 A/B Liquid Silicone Rubber
Vicone High Performance Rubber VicoFluor™ 57FK-GR High Performance Fluoroelastomer Rubber

PWACK9152 / 204681

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.