MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik HF10 Extra-Fine Cemented Carbide for Metal Forming Applications  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: SANDVIK Grade H10F has been developed to meet the exacting demands placed on solid carbide tooling by modern technology.

SANDVIK extra-fine grain cemented car bide grades are true sub micron grain size tungsten carbide alloys with a carbide grain size of 0.8 µm, which is precisely controlled.

This grade offers an excellent combination of strength and toughness. In addition, a special additive maximizes corrosion resistance without loss of toughness.

Features:

  • 10% cobalt and 90% tungsten carbide (WC).
  • High toughness.
  • Applications in the ISO K20/K30 range.
  • Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 14.45 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell A 92.1
    Hardness, Vickers 160030
    Flexural Strength 4300 MPaTransverse Rupture; ISO 3327
    Compressive Strength 6250 MPa
     
    Component Elements PropertiesOriginal ValueComments
    Cobalt, Co 10 %
    WC 90 %
     
    Descriptive Properties
    Corrosion Resistance, 1-105
    Wear Resistance, 0-105

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Sandvik DZ05 Extra-Fine Cemented Carbide for Metal Forming Applications
    Sandvik PN90 Nano-Series Cemented Carbide for Metal Forming Applications
    Sandvik H11N Cemented Carbide for Metal Forming Applications
    Sandvik DZ05 Cemented Carbide for Woodworking
    Sandvik H6N Cemented Carbide for Metal Forming Applications

    NSANDV048 / 18942

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.