MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik DZ05 Extra-Fine Cemented Carbide for Metal Forming Applications  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: Sandvik’s extra fine grained Cemented Carbide grade DZ05 has been developed to meet the high demands modern metal forming sets to Cemented Carbide tools. The very fine grain size means that a superior quality of the cutting edge can be achieved. The binder in the grade is alloyed to improve corrosion resistance.

Features:

  • Extra fine grain cemented carbide grade.
  • Very high wear resistance.
  • Superior cutting edge quality.
  • Improved corrosion and oxidation resistance.
  • (Rather sensitive to brazing and grinding stresses. Brazing and grinding should be carried out under optimum conditions).

    Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 15.0 g/cc0.542 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell A 93.893.8
    Hardness, Vickers 1900190030
    Flexural Strength 2300 MPa334000 psiTransverse Rupture; ISO 3327
     
    Descriptive Properties
    Corrosion Resistance, 1-108
    Wear Resistance, 0-109

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Sandvik DZ05 Cemented Carbide for Woodworking
    Sandvik HF10 Extra-Fine Cemented Carbide for Metal Forming Applications
    Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
    Sandvik H3F Cemented Carbide for Metal Forming Applications
    Overview of materials for Low Alloy Steel

    NSANDV047 / 18941

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.