MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow VORANOL™ 4703 Polyether Polyol
Categories: Polymer; Thermoset

Material Notes: VORANOL™ 4703 polyether polyol is a nominal 5000 molecular weight, high reactivity capped triol. It has a high primary hydroxyl content making it suitable for use in making all types of high resiliency (HR) foam.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.028 g/cc
pH 7.5 - 9.3(1 Water / 10 Methanol)
Viscosity Measure 65 cSt
@Temperature 98.9 °C
 440 cSt
@Temperature 37.8 °C
 855 cSt
@Temperature 25.0 °C
 4600 cSt
@Temperature 0.000 °C
Maximum Moisture Content 0.050wt% water
Vapor Pressure <= 0.0100 torr
ASTM Color <= 50APHA
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.93 J/g-°C
@Temperature 20.0 °C
 2.03 J/g-°C
@Temperature 65.0 °C
 2.13 J/g-°C
@Temperature 100 °C
Thermal Conductivity 0.000306 cal cm/sec-cm²-°C
@Temperature 100 °C
 0.000335 cal cm/sec-cm²-°C
@Temperature 65.0 °C
 0.000368 cal cm/sec-cm²-°C
@Temperature 35.0 °C
Flash Point 224 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4546
 
Descriptive Properties
Hydroxyl Number mg KOH/g32 - 36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow VORANOL™ 4701C Polyether Polyol
Dow VORANOL™ 4701 Polyether Polyol
Dow VORANOL™ 4240 Polyether Polyol
Dow VORANATE™ T-80 toluene diisocyanate (TDI)
Dow VORANOL™ 4815 Polyether Polyol

PDOW1472 / 30690

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.