MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Rynite® 545 BK504 PET-GF45
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 50% Glass Reinforced

Material Notes: 45% Glass Reinforced Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.70 g/cc0.0614 lb/in³ISO 1183
Viscosity Number 55 cm³/g0.55 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 175 MPa25400 psiISO 527-1/-2
Elongation at Break 1.9 %1.9 %ISO 527-1/-2
Tensile Modulus 15.5 GPa2250 ksiISO 527-1/-2
Flexural Modulus 14.0 GPa2030 ksiISO 178
Poissons Ratio 0.330.33
Charpy Impact Unnotched 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 62631-3-2
Dielectric Constant  4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 32.0 kV/mm813 kV/inIEC 60243-1
Dissipation Factor  0.0136
@Frequency 1e+6 Hz
0.0136
@Frequency 1e+6 Hz
IEC 62631-2-1
 0.0214
@Frequency 100 Hz
0.0214
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 225 V225 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C9.44 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 85.0 µm/m-°C47.2 µin/in-°FISO 11359-1/-2
Melting Point 249 °C480 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 230 °C446 °FISO 75-1/-2
Glass Transition Temp, Tg 90.0 °C194 °F10°C/min; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 °C545 °FOptimum, Injection
 280 - 300 °C536 - 572 °FRange, Injection
Mold Temperature 120 °C248 °FOptimum, Injection
 110 - 130 °C230 - 266 °FInjection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %<= 0.020 %Injection
Hold Pressure >= 80.0 MPa>= 11600 psiInjection
 
Descriptive Properties
Back pressureAs low as possible
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0G-value (condensate); ISO 6452
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PET-GF45<ISO 11469
PolymerPET-GF45
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPET-GF45ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 1108 Polyethylene Terephthalate (PET), Glass Fiber
Celanese Rynite® 545 NC010 PET-GF45
Celanese Rynite® 408 NC010 PET
BASF Petra® 140 45% Glass Filled PET
Covestro Petlon® DP3-1027 Semi-Crystalline PET, 45% Glass Fiber

PDSX5262 / 197902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.