MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Guarniflon TENFIL TF 400 Polytetrafluoroethylene Thread Sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: TENFIL TF400 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fittings and threaded joints of different kinds of pipes.
UL 1356 approved for use with METHANE, BUTANE, PROPANE, NATURAL GAS (GPL).

Information provided by Guarniflon®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 50 - 55 %50 - 55 %
pH 4.0 - 6.04.0 - 6.0
Brookfield Viscosity 11000 - 13000 cP11000 - 13000 cP
Surface Tension 38 dynes/cm38 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Boiling Point 100 °C212 °F
Clash Berg Stiffness Temperature 0.000 °C32.0 °F
 
Processing PropertiesMetricEnglishComments
Dry Time 1.00 hour
@Temperature 20.0 °C
1.00 hour
@Temperature 68.0 °F
Drying Air Flow Rate  9000 l/min
@Temperature 80.0 °C,
Time 80.0 sec
318 ft³/min (CFM)
@Temperature 176 °F,
Time 0.0222 hour
 9000 l/min
@Temperature 50.0 °C,
Time 120 sec
318 ft³/min (CFM)
@Temperature 122 °F,
Time 0.0333 hour
Shelf Life 12.0 Month
@Temperature 4.00 - 35.0 °C
12.0 Month
@Temperature 39.2 - 95.0 °F
 
Descriptive Properties
Chemical ResistanceAlcoholGood
 Aliphatic SolventsGood
 Aromatic SolventsModerate
 EsterModerate
 GlycolsGood
 GreaseGood
 KetonesModerate
 OilsGood
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant
Evonik SILIKOFTAL® HTF Silicone Polyester Resin
Shandong Dongyue Shenzhou New Material Co DS603B Fluorinated Ethylene Propylene Dispersion (DS603A/B)
Shandong Dongyue Polymer DF-302 PTFE Aqueous Dispersion 60%
Shandong Dongyue Polymer DF-301 PTFE Aqueous Dispersion 60%

PGUARN027 / 142760

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.