MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CoorsTek PlasmaPure-UC™ 99.9% Alumina
Categories: Ceramic; Oxide; Aluminum Oxide

Key Words: Al2O3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.94 g/ccASTM-C 20
Particle Size 3.0 µmAverage Crystal Size; THIN-SECTION
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 45 N 85
Modulus of Elasticity 386 GPaASTM-C848
Flexural Strength 414 MPaMOR; ASTM-F417
Compressive Strength 2930 MPaASTM-C773
Poissons Ratio 0.24ASTM-C848
Fracture Toughness 4.00 - 5.00 MPa-m½KIC; Notched Beam
Shear Modulus 156 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.10e+7 ohm-cm
@Temperature 1000 °C
ASTM-D1829
 3.30e+12 ohm-cm
@Temperature 500 °C
ASTM-D1829
 >= 1.00e+14 ohm-cm
@Temperature 25.0 °C
ASTM-D1829
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.20 µm/m-°C
@Temperature 25.0 - 1000 °C
ASTM-C372
Thermal Conductivity 31.0 W/m-KASTM-C408
Maximum Service Temperature, Air 1750 °CNO-LOAD COND.
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 99.9 %
 
Descriptive Properties
ColorIvory
Thermal Shock Resistance (°C)200 ΔTc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alumina, alpha Al2O3, 99.5%
CoorsTek UltraSiC™ SC-30 Direct Sintered Silicon Carbide
Aluminum Nitride, AlN
CoorsTek PlasmaPure™ AD-998 Alumina (nom. 99.8% Al2O3)
Corning Macor® Machinable Glass Ceramic

CCOOR903 / 104607

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.