MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polygon Composites Polylube® IFR Backed Bearing high load, low friction composite bearings
Categories: Polymer

Material Notes: The PolyLube® IFR backed bearing can withstand static loads of approximately 70,000 PSI and 30,000 PSI under dynamic loading. At these loading levels, minimum distortion will occur. For dry running applications, the maximum speed is approximately 10 surface feet per minute. The typical average design pressure for high duty cycle applications is 10,000 PSI. This bearing’s operating temperature range is ±325°F. Maximum continuous operational surface temperature for the standard formulation is 325°F, depending upon load characteristics. The bearing has been heat stabilized at these temperatures, so that little dimensional change will occur in the bearing during operation. In a free state, the coefficient of expansion of the PolyLube IFR bearing is approximately 7 x 106 in/in/°F, similar to the coefficient of expansion for steel, and actually less than some metals.

Applications: Excellent applications for IFR backed bearings include bearing systems using alloyed bronze, spring-retained, hardened bearings and hardened steel bearings.

Information provided by Polygon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 9.45 ksiAxial
 20.25 ksiHoop
Modulus of Elasticity 970 ksiRadial (wall)
 1620 ksiTorsional Shear
 2100 ksiAxial
 2570 ksiHoop
Compressive Strength 19.75 psiAxial
 20.25 psiHoop
 30.69 psiRadial (wall)
Poissons Ratio 0.25Uxz
 0.36Uxy
 0.51Uxy
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 325 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TriStar TriSteel AC Metal Backed PTFE Bearing System
Polyram RamTal PM1509 Acetal, Low Friction
Polyram PlusTek PA4501G6 Nylon 66, 30% Glass Fiber Reinforced, Low Friction
Polyram PlusTek PA352M6 Nylon 6.6, 30% Low Friction Mineral Filled
Polyplastics Duranex® CN7130 Polybutylene Terephthalate (PBT), Low friction, Low wear, GF filled

PPOLYG07 / 184506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.