MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:
  • Good extrusion characteristics
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a
UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to produce containers up to 20 gallons in size. This resin is also considered a multipurpose blow molding resin designed for the high speed production of blow molded containers used for packaging household industrial chemicals, toiletries and cosmetics, health and medicinal aids. In addition, it can be blow molded into other thin walled parts and houseware items, and also can be extruded into profiles or sheets.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D792
ESCR 100% Igepal® 180 hour
@Temperature 50.0 °C
F50; Molded and tested in accordance with ASTM D4976; ASTM D1693
High Load Melt Index 25 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
Melt Index of Compound 0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break 4500 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield 3400 psiMolded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break 900 %Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield 8.0 %Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus 132000 psi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength 100 ft-lb/in²Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
 
Thermal PropertiesOriginal ValueComments
Melting Point 266 °FDow Method (DSC)
Crystallization Temperature 118 °CDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 144 °FMolded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point 261 °FASTM D1525
Brittleness Temperature <= -76.0 °FMolded and tested in accordance with ASTM D4976; ASTM D746
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® LR590001 High Density Polyethylene
LyondellBasell Petrothene® LR590005 High Density Polyethylene
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE)
Dow UNIVAL™ DMDD-6230 NT 7 High Density Polyethylene Resin (HDPE)
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE)

PDOW1460 / 30678

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.