MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Aluminum 6101-T6
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 6000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A96101; ISO E-AlMgSi; Aluminium 6101-T6; AA6101-T6; Al6101-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.70 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 71AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 94Converted from Brinell Hardness Value
Hardness, Vickers 81Converted from Brinell Hardness Value
Tensile Strength, Ultimate 32.0 ksiAA; Typical
 17.0 MPa
@Temperature 371 °C
 24.0 MPa
@Temperature 316 °C
 33.0 MPa
@Temperature 260 °C
 69.0 MPa
@Temperature 204 °C
 145 MPa
@Temperature 149 °C
 193 MPa
@Temperature 100 °C
 221 MPa
@Temperature 24.0 °C
 234 MPa
@Temperature -28.0 °C
 248 MPa
@Temperature -80.0 °C
 296 MPa
@Temperature -196 °C
Tensile Strength, Yield 28.0 ksiAA; Typical
 12.0 MPa
@Strain 0.2 %,
Temperature 371 °C
 16.0 MPa
@Strain 0.2 %,
Temperature 316 °C
 23.0 MPa
@Strain 0.2 %,
Temperature 260 °C
 48.0 MPa
@Strain 0.2 %,
Temperature 204 °C
 131 MPa
@Strain 0.2 %,
Temperature 149 °C
 172 MPa
@Strain 0.2 %,
Temperature 100 °C
 193 MPa
@Strain 0.2 %,
Temperature 24.0 °C
 200 MPa
@Strain 0.2 %,
Temperature -28.0 °C
 207 MPa
@Strain 0.2 %,
Temperature -80.0 °C
 228 MPa
@Strain 0.2 %,
Temperature -196 °C
Elongation at Break 19 %
@Temperature -28.0 °C
 19 %
@Temperature 24.0 °C
 20 %
@Temperature -80.0 °C
 20 %
@Temperature 100 °C
 20 %
@Temperature 149 °C
 24 %
@Temperature -196 °C
 40 %
@Temperature 204 °C
 80 %
@Temperature 260 °C
 100 %
@Temperature 316 °C
 105 %
@Temperature 371 °C
 15 %
@Thickness 1.59 mm
AA; Typical
Modulus of Elasticity 10000 ksiAA; Typical; Average of tension and compression. Compression modulus is about 2% greater than tensile modulus.
Poissons Ratio 0.33Estimated from trends in similar Al alloys.
Machinability 50 %0-100 Scale of Aluminum Alloys
Shear Modulus 26.0 GPaEstimated from similar Al alloys.
Shear Strength 20.0 ksiAA; Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 18.0 ohm-cir-mil/ft
@Temperature 20.0 °C
AA; Typical
 
Thermal PropertiesOriginal ValueComments
CTE, linear 13.0 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 21.7 µm/m-°C
@Temperature -50.0 - 20.0 °C
 23.5 µm/m-°C
@Temperature 20.0 - 100 °C
 24.4 µm/m-°C
@Temperature 20.0 - 200 °C
 25.4 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.895 J/g-°C
Thermal Conductivity 1510 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 1150 - 1210 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness
Solidus 1150 °FAA; Typical
Liquidus 1210 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Solution Temperature 950 °Fhold at temperature for 1 hr
Aging Temperature 350 °Fhold at temperature for 6 to 8 hr
Hot-Working Temperature 500 - 950 °F
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 97.6 %As remainder
Boron, B <= 0.06 %
Chromium, Cr <= 0.03 %
Copper, Cu <= 0.10 %
Iron, Fe <= 0.50 %
Magnesium, Mg 0.35 - 0.80 %
Manganese, Mn <= 0.03 %
Other, each <= 0.03 %
Other, total <= 0.10 %
Silicon, Si 0.30 - 0.70 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Aluminum 6063-T6
Aluminum 6101-H111
Aluminum 6101-T61
Aluminum 6351-T6; 6351-T651

MA6101T6 / 9442

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.