MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond EP21TDCF-3 is a two component epoxy for high performance bonding and sealing. It is formulated to cure rapidly at room temperature or faster at elevated temperatures. It has a non-critical mix ratio of one to one by weight or volume. The faster cure allows for a shortened fixture time. Once cured, EP21TDCF-3 has excellent toughness. This gives the system outstanding mechanical shock resistance along with superior thermal cycling capabilities—even when bonding dissimilar substrates. It has a good blend of physical properties including high shear and peel strengths. It bonds well to a wide variety of substrates, including metals, glass, ceramics and many rubbers and plastics. EP21TDCF-3 has the ability to withstand an array of chemicals, including water, fuels and oils, over the service temperature range of -100°F to +250°F. It is 100% reactive without any solvents or diluents. The hardened adhesive is an excellent electrical insulator. The color of Part A is gray and Part B is amber. EP21TDCF-3 is a versatile, exceptionally strong, user friendly system that is widely used in the OEM, aerospace, electronic, electrical and related industries.

Product Advantages:

  • Convenient mixing: non-critical equal weight or volume ratio.
  • Easy application, higher viscosity, thixotropic system.
  • Rapid curing at room temperature; shorter fixturing time.
  • Bonds well to a variety of substrates.
  • Noteworthy resistance to vibration, shock and thermal cycling.
  • Superior shear and peel strengths.
  • Good chemical resistance to water, fuels and oils.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50 - 55
Tensile Strength at Break 7500 psi
@Temperature 23.9 °C
Tensile Modulus 250000 - 300000 psi
@Temperature 23.9 °C
Shear Strength >= 2000 psiAl/Al, Bond
Peel Strength 35.0 pliT-peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Constant 3.8
@Frequency 60 Hz,
Temperature 25.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 23.9 °C
 1.00 - 2.00 hour
@Temperature 93.3 °C
Pot Life 15 - 25 min100 gram mass
Shelf Life 12.0 Month
@Temperature 23.9 °C
in unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1:1by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC
Permabond UV640 UV-curable Adhesive
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White
Henkel Loctite® Ultra Grey® 5999 Flange Sealant
Henkel Loctite® Nuva-Sil® 5084 Sealant

PMASTB323 / 149570

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.