MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours 340 PFA Perfluoroalkoxy Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA)

Material Notes: Combines the processing ease of conventional thermoplastic resins with the excellent properties of PTFE. High chemical resistance, superior electrical properties, high service temperatures, superior high temperature creep resistance, excellent low temperature toughness, and exceptional flame resistance. Processed by conventional melt-extrusion and molding techniques. Resin Characteristics: General purpose; highest flow rate. Uses: Tubing; injection- or blow-molded articles

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Fluoroproducts, in 2015. This specific product was discontinued prior to the formation of Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.12 - 2.17 g/ccASTM D792
Water Absorption <= 0.030 %24 hours; ASTM D570
Melt Flow 14 g/10 minASTM D3307
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ASTM D2240
Tensile Strength, Ultimate 25.0 MPaASTM D3307
 12.0 MPa
@Temperature 250 °C
ASTM D3307
 129 MPa
@Temperature -196 °C
ASTM D1780
Tensile Strength, Yield 13.8 MPaASTM D3307
Elongation at Break 300 %ASTM D3307
 8.0 %
@Temperature -196 °C
ASTM D1708
 480 %
@Temperature 250 °C
ASTM D3307
Flexural Modulus 0.590 GPaASTM D790
 0.0550 GPa
@Temperature 250 °C
ASTM D790
Compressive Strength 24.0 MPa
@Temperature 23.0 °C
ASTM D695
 414 MPa
@Temperature -196 °C
ASTM D695
Compressive Modulus 69.0 GPa
@Temperature 23.0 °C
ASTM D695
 4690 GPa
@Temperature -196 °C
ASTM D695
Izod Impact, Notched NBASTM D256
 0.640 J/cm
@Temperature -196 °C
ASTM D256-72a
Coefficient of Friction, Dynamic 0.213 ft/min; 100 psi; dry vs. steel
 0.21410 ft/min; 100 psi; dry vs. steel
 0.22930 ft/min; 100 psi; dry vs. steel
 0.28950 ft/min; 100 psi; dry vs. steel
K (wear) Factor 694 x 10-10 in³-min/ft-lb-hr50 ft/min; 100 psi; dry vs. steel
 983 x 10-10 in³-min/ft-lb-hr30 ft/min; 100 psi; dry vs. steel
 1591 x 10-10 in³-min/ft-lb-hr3 ft/min; 100 psi; dry vs. steel
 1837 x 10-10 in³-min/ft-lb-hr10 ft/min; 100 psi; dry vs. steel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+17 ohmASTM D257
Dielectric Constant 2.03
@Frequency 60.0 - 1.00e+6 Hz
ASTM D150
Dielectric Strength 80.0 kV/mm
@Thickness 0.0250 mm
Short time; ASTM D149
Dissipation Factor 0.00010
@Frequency 60.0 - 1.00e+6 Hz
ASTM D150
Arc Resistance >= 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 140 µm/m-°C
@Temperature 21.0 - 100 °C
ASTM D696
 170 µm/m-°C
@Temperature 100 - 149 °C
ASTM D696
 210 µm/m-°C
@Temperature 149 - 208 °C
ASTM D696
Specific Heat Capacity 1.172 J/g-°C
@Temperature 100 °C
Melting Point 302 - 310 °CASTM D3418
Maximum Service Temperature, Air 260 °C
Glass Transition Temp, Tg -80.0 °CGlass II
 90.0 °CGlass I
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.35ASTM D542-50
Haze 4.0 %ASTM D1003-52
Transmission, Visible 91 - 96 %
@Thickness 0.0250 mm
0.40 to 0.70 µm
IR Transmittance 96 - 98 %2.5%; 0.70 to 2.40 µm
UV Transmittance 77 - 91 %
@Thickness 0.0250 mm
0.25 to 0.70 µm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 379 - 399 °CCure Temperature
 
Descriptive Properties
20% Hydrochloric Acid Transmission, g/100sq in.<0.02
50% Sodium Hydroxide Transmission, g/100sq in.<.02
Acetic Acid Transmission, g/100sq in.0.41
Acetone Transmission, g/100sq in.0.95
Acetophenone Transmission, g/100sq in.0.5
Benzene Transmission, g/100sq in.0.64
Carbon Tetrachloride Transmission, g/100sq in.0.31
Chemical/Solvent ResistanceExcellent
Ethyl Acetate Transmission, g/100sq in.0.76
Folding Endurance, # cycles, .18-.20 mm15000
Heat of Combustion J/g5300ASTM D240
Hexane Transmission, g/100sq in.0.56
Piperidine Transmission, g/100sq in.0.04
Red Fuming Nitric Acid Transmission, g/100sq in.7.5-1.4
Salt Spray Resistance on aluminum, Hours1000
Sulfuric Acid Transmission, g/100sq in.0.00001
Water Transmission, g/100sq in.0.4
Weather Resistance10Years unaffected in Florida Exposure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours 350 PFA Perfluoroalkoxy Copolymer
Chemours Teflon® PFA Grade 345 Extrusion and Molding Resin
Chemours 100 FEP Fluorinated Ethylene Propylene
Hippe PE 300 Polyethylene
Hippe PE 500 Polyethylene

PDU921 / 33331

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.