MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include heavy produce, textile and frozen food packaging. No Slip, High Antiblock.

Regulatory Status: NA340 resins meet the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "...in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

NA340 resins are processed readily by standard blown film extrusion techniques. A processing melt temperature of 330°-375°F (165°-191°C) is suggested for this resin.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Vinyl Acetate Content 4.0 %
Thickness 1.25 mil
Melt Flow 1.0 g/10 minASTM D1238
Slip Level 0.000 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 340 %ASTM D882
Film Elongation at Break, TD 500 %ASTM D882
Elmendorf Tear Strength MD 180 gASTM D1922
Elmendorf Tear Strength TD 250 gASTM D1922
Dart Drop 112 g/milF50; ASTM D1709
Film Tensile Strength at Break, MD 3700 psiASTM D882
Film Tensile Strength at Break, TD 3100 psiASTM D882
1% Secant Modulus, MD 21000 psiASTM E111
1% Secant Modulus, TD 24000 psiASTM E111
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 95.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %ASTM D1003
Gloss 75 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 °F
Die Opening 0.0635 cm
Blow-up Ratio (BUR) 2.0
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurofoam Evacell EVA 30 EVA + PE Foam
Eurofoam Evacell EVA 100 EVA + PE Foam
ExxonMobil Escorene™ LD 730.09 Blown Ethylene Vinyl Acetate Copolymer
ExxonMobil Escorene™ LD 727.22 Ethylene Vinyl Acetate Copolymer
ExxonMobil Escorene™ LD 726.07 Ethylene Vinyl Acetate Copolymer

PEQU0845 / 104201

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.