MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow UCON™ LB-65 Fluids and Lubricants
Categories: Fluid; Lubricant

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.894 g/cc
@Temperature 100 °C
0.0323 lb/in³
@Temperature 212 °F
 0.942 g/cc
@Temperature 40.0 °C
0.0340 lb/in³
@Temperature 104 °F
 0.960 g/cc
@Temperature 20.0 °C
0.0347 lb/in³
@Temperature 68.0 °F
Viscosity Measurement 1010ISO Viscosity Grade
 8383Index; ASTM D2270, IP 226
 740740@ -18°C, [SUS], Saybolt
Saybolt Viscosity at 100°F 65 SUS65 SUS
Viscosity Measure 58 cSt
@Temperature 0.000 °C
58 cSt
@Temperature 32.0 °F
Saybolt Viscosity at 210°F 35.5 SUS35.5 SUS
Kinematic Viscosity at 40°C (104°F) 11 cSt11 cSt
Kinematic Viscosity at 100°C (212°F) 2.73 cSt2.73 cSt
Molecular Weight 340 g/mol340 g/mol
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.000900 µm/m-°C
@Temperature 55.0 °C
0.000500 µin/in-°F
@Temperature 131 °F
Pour Point -57.0 °C-70.6 °FASTM D97, IP 15
Flash Point 152 °C306 °FPMCC; ASTM D93, IP 34
 221 °C430 °FCOC; ASTM D93, IP 36
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.32811.3281
 
Descriptive Properties
Weight per Gallon7.99 lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phillips 66 Syncon® 22 Synthetic AW Hydraulic Fluid 22
Phillips 66 32 Super Hydraulic Oil
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn Plus™ 3.6 Advanced Polyalphaolefin (PAO) Fluid
ExxonMobil Exxon Hyjet V

PDOW2001 / 183648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.