MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow UCON™ LB-65 Fluids and Lubricants
Categories: Fluid; Lubricant

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.894 g/cc
@Temperature 100 °C
 0.942 g/cc
@Temperature 40.0 °C
 0.960 g/cc
@Temperature 20.0 °C
Viscosity Measurement 10ISO Viscosity Grade
 83Index; ASTM D2270, IP 226
 740@ -18°C, [SUS], Saybolt
Saybolt Viscosity at 100°F 65 SUS
Viscosity Measure 58 cSt
@Temperature 0.000 °C
Saybolt Viscosity at 210°F 35.5 SUS
Kinematic Viscosity at 40°C (104°F) 11 cSt
Kinematic Viscosity at 100°C (212°F) 2.73 cSt
Molecular Weight 340 g/mol
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.000900 µm/m-°C
@Temperature 55.0 °C
Pour Point -57.0 °CASTM D97, IP 15
Flash Point 152 °CPMCC; ASTM D93, IP 34
 221 °CCOC; ASTM D93, IP 36
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.3281
 
Descriptive Properties
Weight per Gallon7.99 lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips 66 Syncon® 22 Synthetic AW Hydraulic Fluid 22
Phillips 66 32 Super Hydraulic Oil
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid
ExxonMobil SpectraSyn Plus™ 3.6 Advanced Polyalphaolefin (PAO) Fluid
ExxonMobil Exxon Hyjet V

PDOW2001 / 183648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.