MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EF923 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose packaging. It is also suggested for heat-sealing treated-to-treated film surfaces and where good clarity is important.

    Application/Uses
  • Bread bags
  • Food packaging
  • Food contact applications
  • Produce bags
  • Industrial packaging

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Good balance of properties
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccASTM D1505
Thickness 1.50 mil
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 250 %ASTM D882
Film Elongation at Break, TD 750 %ASTM D882
Dart Drop Test 100 gASTM D1709
Film Tensile Strength at Break, MD 3800 psiASTM D882
Film Tensile Strength at Break, TD 2700 psiASTM D882
1% Secant Modulus, MD 27000 psiASTM D882
1% Secant Modulus, TD 32000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 6.0 %ASTM D1003
Gloss 70 %at 45º; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 380 °Fwith BUR of 2.4:1 or higher
Blow-up Ratio (BUR) 2.4
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene
LyondellBasell Petrothene® NA345184 Low Density Polyethylene (Film Extrusion)
Westlake EB412 Low Density Polyethylene
Chevron Phillips 4610 LDPE High Clarity, Bakery Packaging Film Resin
Borealis Himod™ FT7324 LDPE for Film

PWESF075 / 84512

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.