MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® Resist 65 Acrylic Sheet
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Optical Sheet

Material Notes: Continuously manufactured ACRYLITE® Resist sheet is a versatile, thermoplastic material developed for the retail display and glazing markets as well as other markets requiring strength, appearance and weatherability. High optical quality ACRYLITE® Resist sheet provides the beautiful look of acrylic with much greater impact strength for durability during manufacturing, shipping, and in-store use. Rigid, tough, and lightweight, ACRYLITE® Resist is easily fabricated and machined, including cutting, routing, forming, and cementing. ACRYLITE® Resist is ideal for use in:
  • P-O-P Displays
  • Store Fixtures
  • Glazing
  • General Fabrication

Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccASTM D729
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70ASTM D785
Tensile Strength, Yield 46.2 MPaASTM D638
Elongation at Yield 6.6 %ASTM D638
Tensile Modulus 2.20 GPaASTM D638
Flexural Strength 82.7 MPaASTM D790
Flexural Modulus 2.06 GPa
Izod Impact, Notched (ISO) 0.750 kJ/m²ASTM D256
Gardner Impact 40.0 in-lbASTM D3029
Impact 866J/m Charpy Impact; ASTM D5942-97
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µin/in-°FASTM D969
Maximum Service Temperature, Air 71.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °CASTM D648
Vicat Softening Point 99.0 °CASTM D1525
Smoke Density 0.022
@Thickness 1.50 mm
 0.038
@Thickness 6.00 mm
Ignition Temperature 399 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ASTM D542
Gloss 140 %20°; ASTM D523
Transmission, Visible 91 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 1837 MAS081 Polycarbonate
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Covestro Makrolon® 2608 Polycarbonate
Overview of materials for Polycarbonate, Impact Modified
A. Schulman Diamond DIAMALOY 1418EF Polycarbonate/Polyester Alloy

PEVONIL052 / 196256

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.