MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical HF380U ABS, High Flow
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Feature: Injection Molding, High Flow, Good Weatherability

Application: Electric & Electronic Products, Miscellaneous Goods)

CAS No. 9003-56-9

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 43 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 106ASTM D785
Tensile Strength, Yield 450 kg(f)/cm²
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Break 40 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Tensile Modulus 21900 kg(f)/cm²
@Thickness 3.20 mm
1 mm/min; ASTM D638
Flexural Yield Strength 720 kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Flexural Modulus 24500 kg(f)/cm²
@Thickness 3.20 mm
15 mm/min; ASTM D790
Izod Impact, Notched 25.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 27.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 12.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
 12.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cm
Dielectric Strength 34.0 kV/mm
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 400 - 600 VSolution A; IEC 60112
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
 15 - 30 sec
@Thickness >=3.00 mm
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 1.50 mm
 >= 120 arcs
@Thickness 3.00 mm
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
 89.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 94.0 °C
@Load 5.00 kg
50°C/h; ASTM D1525
UL RTI, Electrical 60.0 °C
@Thickness >=1.50 mm
UL 746B
 60.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 60.0 °C
@Thickness >=1.50 mm
UL 746B
 60.0 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 60.0 °C
@Thickness >=1.50 mm
UL 746B
 60.0 °C
@Thickness >=3.00 mm
Flammability, UL94 HB
@Thickness >=1.50 mm
 HB
@Thickness >=3.00 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 180 - 200 °CInjection Molding
Middle Barrel Temperature 190 - 210 °CInjection Molding
Front Barrel Temperature 200 - 220 °CInjection Molding
Nozzle Temperature 200 - 230 °CInjection Molding
Melt Temperature 210 - 240 °CInjection Molding
Mold Temperature 40.0 - 70.0 °CInjection Molding
Drying Temperature 80.0 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Back Pressure 29.4 - 58.8 MPaInjection Molding
Screw Speed 30 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical HF380NS ABS, High Flow, General Anti-Static
LG Chemical HF380G ABS, High Flow
LG Chemical HF380XC ABS, High Flow, High Surface Gloss
LG Chemical HG193S ABS, High Flow, Chemical Resistance
LG Chemical HF350U ABS, High Flow

PLAY008 / 148016

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.