MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Diamond, Synthetic
Categories: Carbon; Diamond

Key Words: Diamonds, Carbon, C
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.20 - 3.52 g/cc
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 54 - 84in GPa
Vickers Microhardness 88 - 108GPa; Type 1b
 95 - 131
 108 - 145GPa; Type 11a
Modulus of Elasticity 800 - 925 GPa
Compressive Strength 4500 - 5800 MPa
Poissons Ratio 0.20
Fracture Toughness 6.00 - 10.7 MPa-m½
Shear Modulus 333 - 385 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2000 W/m-K
 
Descriptive Properties
ColorClearImpurities (i.e. Nitrogen) and irradiation can change color to yellow, green, blue, pink, or brown.
Crystal StructureCubicDiamond - Space Group Fd3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Diamond, Natural
Diamond, Polycrystalline
Diamond, thin film
Silicon Carbide, CVD
BACT DLC Diamond-Like Coating

CDiamB / 772

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.