MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Glass Fiber Filled, Flame Retardant

Material Notes: Description: Ultramid 8232G HS FR is a 25% glass fiber reinforced, heat stabilized, flame retardant PA6 injection molding compound exhibiting excellent melt stability characteristics. It combines flame retardant ability with an excellent balance of high strength, stiffness and heat distortion temperature.

Applications: connectors, terminal blocks, switches and receptacles, coil bobbins, and appliance housing

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccASTM D792
Moisture Absorption at Equilibrium 0.90 %24 hour; ASTM D570
 1.1 %50% RH; ASTM D570
 4.0 %Saturation; ASTM D570
Linear Mold Shrinkage 0.00762 cm/cm1/8" bar
 
Thermal PropertiesOriginal ValueComments
UL RTI, Electrical 130 °C
@Thickness 2.50 mm
746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 2.50 mm
746B
UL RTI, Mechanical without Impact 115 °C
@Thickness 2.50 mm
746B
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 290 °C
Mold Temperature 80.0 - 95.0 °C
Dry Time 2 - 4 hour
Moisture Content <= 0.15 %
 
Descriptive Properties
ColorWhite to gray
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8232G HS FR 25% Glass Fiber Fire Retardant PA6 (Dry)
BASF Capron® 8232G HS FR 25% Glass-Filled Nylon 6 (Dry)
Pasargad Polymer Peyvand Pasamid 3P-H1130W Nylon 6, 30% Glass Fiber Reinforced
A. Schulman Diamond DIAMALOY 730 ABS/PC Alloy, Flame Retardant
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry)

PBASG0416 / 132049

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.