MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Lescalloy® 4330+V VAC-ARC High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: LESCALLOY 4330+V VAC-ARC steel is a modification of 4330 steel with hardenability and other properties improved by the addition of vanadium. It is a low alloy steel capable of being heat treated to high strength levels. The alloy is primarily used in the 220 to 240 ksi (1517-1655 MPa) strength range. The comparatively low carbon content of the alloy makes it particularly useful in applications involving shock loading or stress concentration. LESCALLOY 4330+V VAC-ARC steel is produced by the vacuum consumable electrode melting process to provide optimum cleanliness and preferred ingot structure.

Samples were austenitized at 1600°F for 1 hour and oil quenched.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.283 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 47316°C Temper Temperature
 50282°C Temper Temperature
Tensile Strength, Ultimate 225 ksi316°C Temper Temperature
 235 ksi282°C Temper Temperature
Tensile Strength, Yield 1331 MPa316°C Temper Temperature
 1345 MPa282°C Temper Temperature
Elongation at Break 11 %282°C Temper Temperature
 11 %316°C Temper Temperature
Reduction of Area 47 %282°C Temper Temperature
 47 %316°C Temper Temperature
Notched Tensile Strength 2048 MPaKt7; 316°C Temper Temperature
 2083 MPaKt7; 282°C Temper Temperature
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.160 BTU/lb-°F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.30 %
Chromium, Cr 0.85 %
Iron, Fe 95.43 %
Manganese, Mn 0.85 %
Molybdenum, Mo 0.40 %
Nickel, Ni 1.8 %
Silicon, Si 0.30 %
Vanadium, V 0.070 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Astralloy 4330 V-Mod Alloy Steel Round Bars
MetalTek WC 6 Cast UNS J24054 Alloy Steel
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT
Latrobe Lescalloy® 4340 VAC-ARC ; 3.5" round High Strength Alloy Steel

NTIMK023 / 19371

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.