MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Murtfeldt Murpec® Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: In comparison with other thermoplastics, Murpec® has an exceptionally low thermal expansion coefficient. This property provides optimum dimensional stability and means that dimensions do not change even if used in wet environments. Because of the high glass transition temperature, the material’s rigidity and strength are retained almost in their entirety even at high temperatures.

Special Properties:
• High wear resistance
• Low expansion coefficient
• Electrically isolating
• High temperature resistance
• Flame-resistant
• High compressive strength
• High resistance to energy radiation
• Excellent resistance to chemicals and heating steam
• Approved for use in the food industry (EU and/or FDA)

Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.

Key Words: PEEK
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183-1
Moisture Absorption at Equilibrium 0.20 %
@Temperature 23.0 °C
50% RH
Water Absorption at Saturation 0.45 %
@Temperature 23.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105ISO 2039-2
Hardness, Shore D 87DIN 53505
Ball Indentation Hardness 190 MPaISO 2039-1
Tensile Strength 115 MPaISO 527-1/-2
Elongation at Break 17 %ISO 527-1/-2
Modulus of Elasticity 4.30 GPa
Compressive Yield Strength 38.0 MPa
@Strain 1 %
dry; ISO 604
 75.0 MPa
@Strain 2 %
dry; ISO 604
Charpy Impact Unnotched NBISO 179-1/1eU
 NBISO 179
Charpy Impact, Notched 3.50 kJ/m²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.20
Sand Slurry 0.30µm/km
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+14 ohm-cmIEC 60093
Dielectric Constant 3.2
@Frequency 100 Hz
IEC 60250
 3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 24.0 kV/mmIEC 60243-1
Dielectric Loss Index 0.0010
@Frequency 100 Hz
IEC 60250
 0.0020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
 55.0 µm/m-°C
@Temperature 23.0 - 100 °C
 130 µm/m-°C
@Temperature 150 °C
Melting Point 340 °CISO 11357-1
Maximum Service Temperature, Air 250 °C
@Time 1.80e+7 sec
 310 °C
@Time <=86400 sec
Minimum Service Temperature, Air -50.0 °C
Glass Transition Temp, Tg 143 °CISO 11357-1
Flammability, UL94 V-0
 
Compliance PropertiesOriginal ValueComments
European Food 1935/2004 Yes
FDA Yes
 
Descriptive Properties
ColorNatural/Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Murtfeldt Murpec® SP Polyetheretherketone
Isoflon TFM
Pfluon® 8900G PEEK

PMURT938 / 156585

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.