MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

UCAR Carbon UCAR® CHV Extruded Graphite
Categories: Carbon; Graphite

Material Notes: Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.

Tabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.76 g/cc0.0636 lb/in³
Particle Size <= 1500 µm<= 1500 µm
Ash 1.3 %1.3 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 15.9 MPa2300 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000800 ohm-cm0.000800 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 1.10 µm/m-°C
@Temperature 20.0 - 100 °C
0.611 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 150 W/m-K1040 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Niobium C-103 (WC 103; 89Nb-10Hf-1Ti), Stress Relieved
UCAR Carbon UCAR® CS Extruded Graphite
UCAR Carbon UCAR® CGW Isostatic Molded Graphite
AISI Type 316L Stainless Steel, annealed sheet
UCAR Carbon UCAR® CBY Extruded Graphite

CGRAFT05 / 1171

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.