System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
BASF Ultradur® S 4090 G6 30% Glass Filled PBT
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Material Notes:
Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.
Applications: Plug connectors, housings and sunroof.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.47
g/cc
ISO 1183
Water Absorption
0.40 %
DIN 53495/1L
Moisture Absorption at Equilibrium
0.20 %
23°C/50% R.H.
Viscosity Number
105
cm³/g
ISO 1628
Linear Mold Shrinkage, Flow
0.0010
cm/cm
Sheet
0.0029
cm/cm
60x60x2mm; ISO 294
Linear Mold Shrinkage, Transverse
0.0075
cm/cm
60x60x2mm; ISO 294
0.0075
cm/cm
Sheet
Melt Flow
23.9
g/10 min
@Load 2.16 kg,
Temperature 275 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
164
MPa
ISO 2039-1
Tensile Strength at Break
125
MPa
5mm/min; ISO 527-2
Tensile Strength
65.0
MPa
@Temperature 100 °C
ISO 527
120
MPa
@Temperature 50.0 °C
ISO 527
150
MPa
@Temperature 23.0 °C
ISO 527
195
MPa
@Temperature -40.0 °C
ISO 527
Elongation at Break
2.2 %
5mm/min; ISO 527-2
Modulus of Elasticity
9.70
GPa
ISO 527-2
Flexural Strength
183
MPa
ISO 178
Charpy Impact Unnotched
5.90
J/cm²
ISO 179/1eU
Charpy Impact, Notched
0.900
J/cm²
ISO 179/1eA
Dart Drop, Total Energy
<=
5.00
J
ISO 6603-1
Tensile Creep Modulus, 1000 hours
6700
MPa
ISO 899-1
Electrical Properties
Original Value
Comments
Volume Resistivity
3.00e+15
ohm-cm
IEC 60093
Surface Resistance
1.00e+14
ohm
IEC 60093
Dielectric Constant
3.7
@Frequency 1e+6 Hz
IEC 60250
3.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength
95.0
kV/mm
IEC 243/1
Dissipation Factor
0.0030
@Frequency 100 Hz
IEC 60250
0.018
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index
125
V
Test solution B; IEC 60112
500
V
Test solution A; IEC 60112
Thermal Properties
Original Value
Comments
Specific Heat Capacity
1.50
J/g-°C
IEC 1006
Thermal Conductivity
0.290
W/m-K
DIN 52612
Melting Point
220
-
225
°C
Maximum Service Temperature, Air
110
°C
at 50% loss of tensile strength after 20000h; IEC 216-1
140
°C
at 50% loss of tensile strength after 5000h; IEC 216-1
170
°C
Deflection Temperature at 0.46 MPa (66 psi)
210
°C
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi)
175
°C
ISO 75-2
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.800 mm
Flame Spread
<=
100
mm/min
DIN 75200
Glow Wire Test
760
°C
@Thickness 3.00 mm
IEC 695
Processing Properties
Original Value
Comments
Melt Temperature
250
-
275
°C
Injection molding
270
°C
for shrinkage test
Mold Temperature
60.0
-
100
°C
80.0
°C
for shrinkage test
Descriptive Properties
Color
Natural
Commercial Status
Active America
Form
Pellets
Impact Modified
No
Primary Processing Technique
Injection Molding
Processing
Injection Molding
Special characteristic
Heat stabilized or stable to heat
Light stabilized or stable to light
Lubricant
U.V. stabilized or stable to weather
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
BASF Ultradur® B 4300 G6 30% Glass Filled PBT
PTS PBT-30GF 30% Glass Fiber Reinforced PBT
BASF Ultradur® B 4520 PBT
BASF Ultradur® S 4090 G4 20% Glass Filled PBT
Envalior Akulon® K224-G6-FC BK00001 PA6-GF30
PBASF9096 / 84860
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.