MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical EWS LARD OIL Lubricity Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: EWS Lard Oil is an additive that provides excellent lubricity in cutting oils. EWS Lard Oil also provides excellent wetting characteristics that will improve surface finish.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.915 g/cc
@Temperature 25.0 °C
Saybolt Viscosity at 100°F 195 SUS
ASTM Color <= 3.0
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 230 °CCOC
 
Descriptive Properties
% Free Fatty Acid<4as Oleic
Saponification Number195

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dover Chemical PRIME BURNING LARD OIL Lard Oil, Lubricity Additive
Dover Chemical MAYCO BASE 1210 Sulfurized Lard Oil, Non-Staining Sulfurized Additive
Dover Chemical BASE 107 Sulfurized Lard Oil Active Sulfurized Additive
Dover Chemical BASE 101 Sulfurized Lard Oil, Lubricity/Extreme Pressure Additive

WDOVER131 / 217750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.