MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 200-15 Polycarbonate, General Purpose
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Unreinforced, Flame Retardant

Material Notes: CALIBRE® 200-15 Polycarbonate resins produced in to compliance with the applicable FDA and European regulations governing food contact. They provide excellent impact resistance, heat distortion resistance and optical clarity. CALIBRE 200-15 series products are available in 4 additive packages: CALIBRE 200: No mold release or UV stabilizer. CALIBRE 201: Mold release. CALIBRE 202: UV Stabilizer. CALIBRE 203: Mold release and UV stabilizer. (Note that CALIBRE 202 and 203 grades are not available in Europe and do not comply with EU food contact regulations).

Govt. and Industry Standards:

  • US FDA 21 CFR 177.1580
  • CSA
  • Underwriters Laboratory (UL)
  • EU food contact 2011/10/EC
Application:
  • Food processors
  • Beverages containers
  • Food utensils
  • Other packaging applications
Automotive Specifications:
  • GM GMP.PC.015

Data provided by Dow Chemical.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption 0.15 %ISO 62
Moisture Absorption at Equilibrium 0.32 %ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmFlow; ISO 294-4
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 72ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength, Ultimate 71.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 62.1 MPa50 mm/min; ASTM D638
Elongation at Break 150 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
Tensile Modulus 2.34 GPa50 mm/min; ASTM D638
Flexural Strength 96.5 MPaMehotd I (3 point load), 2 mm/min; ASTM D790
 97.0 MPa2 mm/min; ASTM D790
Flexural Modulus 2.40 GPa2 mm/min; ASTM D790
 2.41 GPaMehotd I (3 point load), 2 mm/min; ASTM D790
Izod Impact, Notched 8.50 J/cmASTM D256
Izod Impact, Unnotched NBASTM D256
Izod Impact, Notched (ISO) 83.0 kJ/m²ISO 180/A
Tensile Impact Strength 462 kJ/m²ASTM D1822
Instrumented Impact Total Energy 87.0 J
@Temperature 23.0 °C
3.39 m/sec; ASTM D3763
Abrasion 45[%], Taber; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+18 ohm-cmASTM D257
Dielectric Constant 2.93
@Frequency 60 Hz
ASTM D150
 2.93
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 16.5 kV/mmASTM D149
Dissipation Factor 0.00050
@Frequency 60 Hz
ASTM D150
 0.0017
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 250 V
@Thickness 2.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
ASTM D257
Deflection Temperature at 0.46 MPa (66 psi) 143 °CAnnealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °CUnannealed; ASTM D648
 140 °CAnnealed; ASTM D648
Vicat Softening Point 154 °CISO 306
Flammability, UL94 HB
@Thickness 3.20 mm
 HB
@Thickness 1.60 mm
Oxygen Index 26 %ISO 4589-2
Glow Wire Flammability Index 850 °CIEC 60695-2-13
Ring & Ball Softening Point 125 °CIEC 60335-1
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ASTM D542
Haze 1.0 %ASTM D1003
Transmission, Visible 89 %ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 2608 Polycarbonate
Covestro Apec® 1600 Polycarbonate
Trinseo CALIBRE™ 200 22 Polycarbonate, General Purpose
Trinseo CALIBRE™ 201-22 Polycarbonate Resin
Covestro Apec® 2000 Polycarbonate

PZZDW015 / 34246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.