MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Overview of materials for Phenolic, Novolac, Glass Filled
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 - 2.47 g/cc0.0542 - 0.0892 lb/in³Average value: 1.79 g/cc Grade Count:87
Water Absorption 0.0300 - 1.81 %0.0300 - 1.81 %Average value: 0.118 % Grade Count:60
Linear Mold Shrinkage 0.000500 - 0.00670 cm/cm0.000500 - 0.00670 in/inAverage value: 0.00220 cm/cm Grade Count:80
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 78.0 - 10578.0 - 105Average value: 92.4 Grade Count:16
Hardness, Rockwell M 85.0 - 12085.0 - 120Average value: 111 Grade Count:14
Tensile Strength, Ultimate 34.0 - 145 MPa4930 - 21000 psiAverage value: 84.6 MPa Grade Count:83
Elongation at Break 0.500 - 1.03 %0.500 - 1.03 %Average value: 0.767 % Grade Count:33
Modulus of Elasticity 9.30 - 26.1 GPa1350 - 3790 ksiAverage value: 16.2 GPa Grade Count:44
 11.0 - 11.0 GPa
@Temperature 150 - 150 °C
1600 - 1600 ksi
@Temperature 302 - 302 °F
Average value: 20.8 GPa Grade Count:1
 16.3 - 27.1 GPa
@Temperature -40.0 - 150 °C
2360 - 3930 ksi
@Temperature -40.0 - 302 °F
Average value: 20.8 GPa Grade Count:1
 16.3 - 27.1 GPa
@Strain 0.100 - 0.100 %
2360 - 3930 ksi
@Strain 0.100 - 0.100 %
Average value: 20.8 GPa Grade Count:1
Flexural Yield Strength 74.0 - 325 MPa10700 - 47100 psiAverage value: 159 MPa Grade Count:87
Flexural Modulus 8.60 - 25.0 GPa1250 - 3630 ksiAverage value: 15.7 GPa Grade Count:81
Flexural Strain at Break 1.00 - 1.63 %1.00 - 1.63 %Average value: 1.46 % Grade Count:22
Compressive Yield Strength 110 - 380 MPa16000 - 55100 psiAverage value: 241 MPa Grade Count:84
Poissons Ratio 0.250 - 0.3400.250 - 0.340Average value: 0.305 Grade Count:4
Shear Modulus 3.47 - 10.4 GPa503 - 1510 ksiAverage value: 6.11 GPa Grade Count:3
Izod Impact, Notched 0.209 - 13.5 J/cm0.392 - 25.3 ft-lb/inAverage value: 1.13 J/cm Grade Count:39
Izod Impact, Notched (ISO) 4.00 - 4.50 kJ/m²1.90 - 2.14 ft-lb/in²Average value: 4.17 kJ/m² Grade Count:3
Charpy Impact Unnotched 0.570 - 2.10 J/cm²2.71 - 9.99 ft-lb/in²Average value: 1.33 J/cm² Grade Count:35
Charpy Impact, Notched 0.191 - 0.620 J/cm²0.909 - 2.95 ft-lb/in²Average value: 0.380 J/cm² Grade Count:49
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.20e+11 - 3.82e+15 ohm-cm1.20e+11 - 3.82e+15 ohm-cmAverage value: 2.63e+14 ohm-cm Grade Count:32
Surface Resistance 1.00e+11 - 7.36e+13 ohm1.00e+11 - 7.36e+13 ohmAverage value: 1.61e+13 ohm Grade Count:21
Insulation Resistance 2.00e+7 - 1.00e+14 ohm2.00e+7 - 1.00e+14 ohmAverage value: 6.65e+12 ohm Grade Count:11
Dielectric Constant 4.30 - 7.504.30 - 7.50Average value: 5.46 Grade Count:16
Dielectric Strength 7.90 - 40.0 kV/mm201 - 1020 kV/inAverage value: 18.6 kV/mm Grade Count:73
Dielectric Breakdown  >= 15000 V
@Temperature 90.0 - 90.0 °C
>= 15000 V
@Temperature 194 - 194 °F
Average value: 15000 V Grade Count:1
 >= 15000 V
@Time 20.0 - 60.0 sec
>= 15000 V
@Time 0.00556 - 0.0167 hour
Average value: 15000 V Grade Count:1
Dissipation Factor 0.0150 - 0.1500.0150 - 0.150Average value: 0.0403 Grade Count:16
Arc Resistance 89.0 - 204 sec89.0 - 204 secAverage value: 173 sec Grade Count:32
Comparative Tracking Index 125 - 399 V125 - 399 VAverage value: 182 V Grade Count:38
Hot Wire Ignition, HWI 0.000 - 120 sec0.000 - 120 secAverage value: 60.0 sec Grade Count:5
High Amp Arc Ignition, HAI 15.0 - 120 arcs15.0 - 120 arcsAverage value: 61.2 arcs Grade Count:5
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min0.000 - 0.394 in/minAverage value: 5.00 mm/min Grade Count:5
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.00 - 38.0 µm/m-°C2.78 - 21.1 µin/in-°FAverage value: 19.3 µm/m-°C Grade Count:43
 35.0 - 48.0 µm/m-°C
@Temperature 40.0 - 130 °C
19.4 - 26.7 µin/in-°F
@Temperature 104 - 266 °F
Average value: 41.7 µm/m-°C Grade Count:3
CTE, linear, Transverse to Flow 11.0 - 55.0 µm/m-°C6.11 - 30.6 µin/in-°FAverage value: 39.8 µm/m-°C Grade Count:34
Thermal Conductivity 0.370 - 1.22 W/m-K2.57 - 8.47 BTU-in/hr-ft²-°FAverage value: 0.624 W/m-K Grade Count:15
 0.500 - 0.580 W/m-K
@Temperature 100 - 100 °C
3.47 - 4.03 BTU-in/hr-ft²-°F
@Temperature 212 - 212 °F
Average value: 0.540 W/m-K Grade Count:3
Maximum Service Temperature, Air 150 - 225 °C302 - 437 °FAverage value: 168 °C Grade Count:20
Deflection Temperature at 1.8 MPa (264 psi) 151 - 360 °C304 - 680 °FAverage value: 245 °C Grade Count:73
Deflection Temperature at 8.0 MPa 136 - 195 °C277 - 383 °FAverage value: 168 °C Grade Count:12
UL RTI, Electrical 65.6 - 150 °C150 - 302 °FAverage value: 136 °C Grade Count:6
UL RTI, Mechanical with Impact 150 °C302 °FAverage value: 150 °C Grade Count:6
UL RTI, Mechanical without Impact 150 °C302 °FAverage value: 150 °C Grade Count:5
Flammability, UL94 V-1 - V-0V-1 - V-0Grade Count:43
Oxygen Index 31.0 - 46.0 %31.0 - 46.0 %Average value: 40.5 % Grade Count:4
 
Processing PropertiesMetricEnglishComments
Mold Temperature 155 - 180 °C311 - 356 °FAverage value: 168 °C Grade Count:15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Phenolic; Unreinforced; Molded
Overview of materials for Phenolic, Resole, Glass Fiber Filled
Overview of materials for Phenolic, Novolac, Impact Grade, Filled
Overview of materials for Phenolic, Novolac, Heat Resistant Grade, Filled
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled

O2734 / 78097

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.