MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain Tygon® LP 1500 Low Permeation Fuel Tubing
Categories: Polymer; Thermoplastic

Material Notes: Tygon® LP1500 Low Permeation Fuel Tubing is designed to meet new emission standards.

Applications

  • Fluid power pumps and motors
  • Hand-held lawn and garden power equipment
  • Small engine fuel lines
  • Small utility, farm and construction equipment

Product Features

  • EPA and CARB certified to meet permeation emission standards of 15g/M2/day
  • Robust multi-layer design with barriers to minimize permeation
  • Chemical and fuel resistant inner layer
  • UV resistant outer jacket
  • Wide temperature range from -40° F to 185° F (-40° C to 85° C)
  • Superior clarity and flexibility

Product Benefits

  • Conforms to new government regulatory standards for clean air
  • Highly flexible and kink resistant
  • Clear tubing provides easy observation of fuel flow
  • Higher temperature rating for heat resistance
  • Sub-zero cold temperature impact strength
  • UV resistant outer jacket to prevent premature aging
  • High abrasion, cut and tear resistance for longer service life
  • Tight tolerances for better fitting retention and better seal
  • Compatible with E-10 ethanol blend fuel

Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Water Absorption 0.90 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
@Time 15.0 sec
ASTM D2240
Tensile Strength 5000 psiASTM D412
Elongation at Break 400 %ASTM D412
100% Modulus 1000 psi
@Strain 100 %
ASTM D412
Tear Strength 98.0 kN/mASTM D1004
Compression Set 35 %
@Temperature 70.0 °C,
Time 79200 sec
Method B; ASTM D395
Tensile Set 35 %
@Strain 75 %
ASTM D412
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 185 °F
Minimum Service Temperature, Air -40.0 °FFlexibility

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems
Saint-Gobain Tygon® A-60-N Drinking Water Tubing Formulation
Saint-Gobain Tygon® Noroprene® Chemical Tubing Formulation
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation

PSTGQ919 / 160415

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.