MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cossa Polimeri ESTABLEND 0840 GF Polycarbonate ABS Blend, 20% Glass Filled
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Material Notes: Polycarbonate and Acrylonitrile Butadiene Styrene blend with 20% glass fiber reinforcement

High dimensional stability, high stiffness

Information provided by Cossa Polimeri S.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccASTM D 792
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmASTM D 955
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaASTM D 638
Elongation at Break 3.0 %ASTM D 638
Flexural Modulus 5500 MPaASTM D 790
Izod Impact, Notched 80.0 J/m
@Temperature 0.000 °C
ASTM D 638
 100 J/m
@Temperature 23.0 °C
ASTM D 256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 132 °C
@Load 5.00 kg
50°C/hr; ASTM D 1525
 142 °C
@Load 0.999 kg
50°C/hr; ASTM D 1525
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled
Cossa Polimeri ESTABLEND 0820 GF Polycarbonate ABS Blend, 10% Glass Filled
A. Schulman Diamond ABSPC 9901GF20 Injection Molding Grade, 20% Glass Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled

PCOSSA857 / 156447

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.