MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.

Films manufactured with Flexirene FG 30 are characterized by an optimum balance between mechanical properties (stiffness) and sealing properties.

Main Applications: Flexirene FG 30 is recommended for the production of general purpose film, automatic packaging and food packaging, especially when food is submitted to continuous cooking.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.925 g/ccISO 1183
Thickness 15.0 - 50.0 micronsRecommended
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 13.0 MPaISO 527-3
Film Elongation at Break, MD 600 %ISO 527-3
Film Elongation at Break, TD 800 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50ISO 8295
Elmendorf Tear Strength, MD 2.5475 g/micronISO 6383-2
Elmendorf Tear Strength, TD 18.342 g/micronISO 6383-2
Dart Drop Test 60.0 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 45.0 MPaISO 527-3
Film Tensile Strength at Break, TD 33.0 MPaISO 527-3
1% Secant Modulus, MD 250 MPaISO 527-3
1% Secant Modulus, TD 290 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 124 °CInternal method
Vicat Softening Point 105 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -70.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 13 %ISO 14782
Gloss 50 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LD 07523.BW Low Density Polyethylene Resin
ExxonMobil LD 07523.AC Low Density Polyethylene Resin
ExxonMobil HD 6207 High Density Polyethylene Resin
ExxonMobil HD 5404 High Density Polyethylene Resin
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade)

PENG094 / 124488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.