MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP21TDCAOHT Two Component Thermally Conductive, Electrically Insulative Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: EP21TDCAOHT is a two component, flexibilized, thermally conductive epoxy adhesive that will cure at room temperature, or more rapidly at elevated temperature. It is a good adhesive sealant, with high peel strength and tensile lap shear. It has a very convenient mix ratio(1:1), weight or volume, and is serviceable over an exceptionally wide temperature range of -100 to 400°F. As a flexibilized system, it is an ideal adhesive for bond dissimilar substrates when thermal conductivity is needed. EP21TDCAOHT has superior thermal and mechanical shock resistance and is readily thermally cyclable.

Product Advantages:

  • Convenient mixing: non-critical equal weight or volume ratio.
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly; no drip application feature.
  • Versatile cure schedules: ambient temperature cures or fast elevated temperature cures as required.
  • High shear and peel strength, ideal for dissimilar substrates.
  • Good durability, thermal shock and chemical resistance.
  • High thermal conductivity with excellent electrical insulation properties.
  • Very wide service temperature range -100 to 350°F.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Shear Strength 1000 psiafter 30 days water immersion, Al/Al, Bond
 1100 psiAl/Al, Bond
Peel Strength 5.00 - 10.0 pliT-peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 9.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -100 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 48.0 hour85% of maximum strength developed within
Pot Life 45 - 60 min1 quart mass
 60 - 90 min200 gram mass
Shelf Life 6.00 Month
@Temperature 23.9 °C
in unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1/1by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP21TDC-2AN Two Component, Flexibilized, Highly Thermally Conductive, Electrically Insulating Epoxy Resin
Rogers Arlon Thermabond® 99A30N008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Master Bond Supreme 11AOHT Thermally Conductive, Heat Resistant Epoxy System
Master Bond EP21TDCANHT Two Component Thermally Conductive, Electrically Insulative Epoxy Adhesive
Master Bond EP21AOLV-2LO Two Part, Thermally Conductive and Electrically Insulative Epoxy

PMASTB322 / 149569

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.