System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Ecomass® 4703ZD95 Tungsten Filled Polyurethane
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications
High Specific Gravity
Tungsten Powder Filled Polyurethane (TPU)
Flexible
Information provided by Technical Polymers
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
10.0
g/cc
ASTM D792
Linear Mold Shrinkage
0.0030
-
0.0050
cm/cm
ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
2000
psi
ASTM D638
Elongation at Break
12 %
ASTM D638
Tensile Modulus
96000
psi
ASTM D638
Flexural Strength
3350
psi
ASTM D790
Flexural Modulus
116000
psi
ASTM D790
Izod Impact, Notched
5.00
ft-lb/in
ASTM D256
Electrical Properties
Original Value
Comments
Surface Resistivity per Square
0.20
ohm
ASTM D257
Processing Properties
Original Value
Comments
Melt Temperature
400
-
430
°F
Mold Temperature
50.0
-
80.0
°F
Drying Temperature
200
°F
then reduce to 160°F
Dry Time
2
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Ecomass® 4703ZD84 Tungsten Filled Polyurethane
Ecomass® Ecomass® 5033ZG87 SS/Tungsten Powder filled Styrene Isoprene Styrene (SIS)
Ecomass® Ecomass® 4150TU96 Tungsten Powder filled Polyphenylene Sulfide (PPS)
Ecomass® 720ZD88 Tungsten Filled ABS
Ecomass® 3608TU96 Tungsten Filled Polyethylene
PECOM64 / 35474
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.