MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Casico™ FR4820 Natural Low Smoke Zero Halogen Flame Retardant Insulation Compound for Building Energy Cables  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Casico™ FR4820 is a thermoplastic, low smoke zero halogen (LSZH) flame retardant, UV stabilized, natural insulation compound combining with excellent extrusion properties. It is based on the novel technology, Casico™, containing inorganic filler and a novel char-forming additive which confer flame retardancy with very limited smoke generation. Applications: 70°C rated insulation for building wires (installation cables), flexible cords, and power cables. It can be used in areas sensitive to smoke or corrosive and toxic combustion products. Casico™ FR4820 is stabilized for use in contact with copper. Specifications: Casico™ FR4820 in combination meets these applicable requirements when processed using extrusion practice and testing procedure: EN 50292-2-26; EN 50363-7 TI6; and EN 50363-7 TI7.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/cccompound; ISO 1872-2/ISO 1183
Water Absorption 0.0087 %
@Time 1.21e+6 sec
70°C, .1mg/cm2; IEC 60811-1-3
Melt Flow 0.90 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 4015s; ISO 868
Tensile Strength at Break <= 2.60 MPaafter aging, 240h, 100°C; or UV aging
 13.0 MPa50mm/min; IEC 60811-1-1
Elongation at Break <= 110 %after aging, 240h, 100°C; or UV aging
 550 %ISO 527
Flexural Modulus 215 MPaISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmIEC 60093
Dielectric Strength <= 20.0 kV/mmIEC 60243
Dielectric Breakdown 36000 VISO 6722
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °CISO 4589-3
Brittleness Temperature <= -60.0 °CISO 974
Smoke Density 49NBS 6 min; flaming mode; 76x76x.7mm
 104NBS 20 min; non-flaming mode; 76x76x.7mm
Oxygen Index 27 %
 
Processing PropertiesOriginal ValueComments
Zone 1 160 °C
Zone 2 170 °C
Zone 3 180 °C
Zone 4 190 °C
Die Temperature 190 °C
 
Descriptive Properties
Average Heat Release, kW/m2244ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
CO, kg/dm30.023ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
CO2, kg/dm31.7ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
Cold Bend (-40°C)PassIEC 60811-1-4
Cold Impact(-40°C)PassIEC 60811-1-4
Corrosivity of Combustion Fumes1.5IEC 60754-2
Dielectric DurationPassIEC 60227-2/2.3
Heat Combustion, MJ/dm329ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
High Temperature Pressure Test, %< 50%90°C, 4 hours, IEC 60811-1-4
Ignition Time, sec125ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
Max Heat Release, kW/m2400ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque
Smoke Obscuration, m2/dmm3520ISO 5660; Cone Calorimeter (heat flux 35 kW/m2, 3mm plaque

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis FR4810 Low Smoke Zero Halogen Flame Retardant Jacketing Compound
Borealis Casico™ FR6083 Reduced Fire Hazard Jacketing Compound
BASF Elastollan® 1154 D FHF TPUR Flame Retardant Halogen Free
Fainplast Compounds Hax™ HFX 519 Crosslinkable HFFR Cable Compound
Fainplast Compounds Hax™ HFX 521 Crosslinkable HFFR Cable Compound

PBOREA400 / 108659

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.