MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Avient Therma-Tech™ NN-5000C TC Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of thermoplastics. These materials provide the benefits of proprietary conductive additive technologies and the performance of select engineering thermoplastic resins. Therma-Tech compounds have been shown to improve thermal conductivity up to 100-times that of conventional plastics and can be used in a wide range of thermal management applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/ccASTM D792
Water Absorption 0.40 %
@Thickness 3.18 mm,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 51.0 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 0.80 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 14500 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 88.9 MPaASTM D790
Flexural Modulus 11200 MPaASTM D790
Izod Impact, Notched 32.0 J/m
@Thickness 6.35 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 - 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+13 - 1.00e+14 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 5.50 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 266 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
@Thickness 6.35 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 282 - 299 °C
Mold Temperature 65.6 - 93.3 °C
 
Descriptive Properties
FeaturesElectrically Insulating
 Thermally Conductive
FormsPellets
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Automotive Under the Hood
 Consumer Applications
 Electrical/Electronic Applications
 Housings
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® T1 GF 40 (3464) PPA Dry, 40% Glass Filled
EMS-Grivory Grivory® HT1V-4 FWA black 9225 PA6T/6I-GF40
RTP Company RTP 207E  Amorphous Nylon (Am. PA) Glass Fiber 40%
Avient Therma-Tech™ NJC-7500 TC Nylon 12
Avient Therma-Tech™ NJC-6000 TC Nylon 12

PH1PN9508 / 103344

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.