MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zenite® 6130LX WT010 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: Zenite® 6130LX WT010 is a 30% glass reinforced, lubricated liquid crystal polymer resin with improved weldline strength and a heat deflection temperature of 280°C.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.66 g/ccISO 1183
Filler Content 30 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 145 MPaISO 527
Elongation at Break 2.0 %ISO 527
Tensile Modulus 15000 MPa
@Temperature 23.0 °C
ISO 527
Flexural Strength 220 MPa
@Temperature 23.0 °C
ISO 178
Flexural Modulus 12500 MPa
@Temperature 23.0 °C
ISO 178
Charpy Impact, Notched 2.00 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 249 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear -1.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 260 °C
ISO 11359-1/-2
 3.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 3.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 5.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 5.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 6.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 6.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 260 °C
ISO 11359-1/-2
 6.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 48.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2; 2mm
 55.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2; 4mm
 68.0 µm/m-°C
@Temperature -40.0 - 260 °C
ISO 11359-1/-2; 2mm
 76.0 µm/m-°C
@Temperature -40.0 - 260 °C
ISO 11359-1/-2; 4mm
 55.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 62.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 71.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 80.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 80.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
 92.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
Melting Point 335 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 280 °CISO 75-1/-2
UL RTI, Electrical 240 °C
@Thickness 1.50 mm
UL 746B
 240 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical with Impact 220 °C
@Thickness 1.50 mm
UL 746B
 220 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical without Impact 240 °C
@Thickness 1.50 mm
UL 746B
 240 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
UL94
 V-0
@Thickness 3.00 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
UL94
Glow Wire Ignition Temperature 960 °C
@Thickness 1.50 mm
IEC 60695-2-13
 960 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 355 °COptimum
 350 - 360 °C
Mold Temperature 80.0 °COptimum
 40.0 - 150 °C
Drying Temperature 150 °C
Dry Time 3 hourDehumidified Dryer
Moisture Content <= 0.010 %
 
Descriptive Properties
ColorWhite
Drying RecommendedYes
FillerGlass Reinforced
FormsPellets
GenericLCP
Part Marking Code>LCP-GF30<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Flame Retardant Resins
 Glass Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-GF30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zenite® 6130 WT010 30% GF LCP (Extended Tabular Temperature Data)
Celanese Zenite® 7130 WT010 LCP (Extended Tabular Temperature Data)
Celanese ZENITE 5130L LCP, 30% Glass Reinforced
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese ZENITE 6130LX LCP, 30% Glass Reinforced

PHCQ538b / 89592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.