MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) SILCOLAPSE® 137 Antifoam
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: SILCOLAPSE 137 is a non-ionic aqueous emulsion containing dimethylpolysiloxane, and is highly effective for control and elimination of foam in aqueous media. Active ingredient concentration is 10%. This product is highly effective in aqueous media and subjected to extreme agitation, even at temperatures of over 80ºC. It is active in extreme pH conditions. SILCOLAPSE 137 is exclusively designed for industrial use.

Applications: SILCOLAPSE 137 is particularly suitable for use in industrial processes requiring the elimination or control of foam in aqueous media and subjected to extreme agitation, such as:

  • Extraction, distillation and dehydration processes.
  • Manufacture of adhesives and glues.
  • ?Manufacture of soaps and detergents.
  • Agrochemical formulations.
  • Manufacture of ethylene oxide and propylene oxide.
  • Formulation of natural and synthetic latex.
  • Effluent treatment.
Advantages:
  • Easy dispersion in aqueous media.
  • High foam control capability in a wide variety of foaming media.
  • Homogeneous and stable emulsion.
  • Chemically inert with regards to the medium to be defoamed.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
pH 4.5
Viscosity 2000 cP
Storage Temperature 5.00 - 30.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
Appearancemilky liquid
Colorwhite
Content10% Active
Diluentswater
Emulsifier typenon-ionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Atom Adhesives AA-GREASE 04 Epoxy Adhesive
Silberline Silvet® 410-20-P
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA)
Overview of materials for Methacrylate Adhesive
NeoGraf GRAFOIL® GTH Standard Fluid Sealing Adhesive-Backed Tape, Gasket and Thread Tape

PBLUST013 / 190989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.