MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Omni Plastics OmniPro™ TPO 20M HC Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: High impact resistance, easy flow, enhanced clarity; values are based on natural or black materials unless otherwise noted.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D792
Melt Flow 18 g/10 minASTM D1248
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 19.0 MPaASTM D638
Flexural Strength 21.0 MPaASTM D790
Flexural Modulus 758 MPaASTM D790
Izod Impact, Notched 320 J/m
@Thickness 3.17 mm,
Temperature -30.0 °C
ASTM D256
 NB
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C
@Thickness 3.17 mm
ASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Omni Internal Testing
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 400 - 480 °F
Middle Barrel Temperature 420 - 500 °F
Front Barrel Temperature 420 - 500 °F
Nozzle Temperature 420 - 500 °F
Melt Temperature 420 - 500 °F
Mold Temperature 80.0 - 140 °F
Back Pressure 50.0 - 100 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zylog Hipolyene® 1048 X1 Thermoplastic Polyolefin & PP Compound
Solvay Engineered Polymers SEQUEL® 1440LS TPO
Phillips Sumika Marlex® CHN-200 Thermoplastic Polyolefin
Omni Plastics OmniPro™ TPO MF20 HF HSV Thermoplastic Polyolefin
LyondellBasell SEQUEL® 1780 Engineered Polyolefin

POMNI5089 / 185235

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.