MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haysite 14100 Polyester BMC, 15% Glass Reinforced
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: The 14100 series bulk molding compound is an electrical grade material that can be compression, transfer, or injection molded. Offering good mechanical strength and excellent electrical properties, this grade also exhibits low shrink characteristics. The 14100 BMC is recognized by UL with a 94V-0 flame rating at .060" wall thickness.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.89 g/ccASTM D572
Water Absorption 0.10 %ASTM D570
Linear Mold Shrinkage 0.00075 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 41.0 MPa
Flexural Strength 86.0 MPa
Compressive Strength 90.0 MPa
Izod Impact, Notched 1.90 J/cmedgewise; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 16.0 kV/mmPerpendicular (ASTM D149), Short Time
Dissipation Factor 0.033
@Frequency 60 Hz
ASTM D150
Arc Resistance 192 secASTM D495
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 130 °Ctemperature rating
Flammability, UL94 V-0File No.E-27875

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 50 wt.% glass
Plenco 1500 Polyester, Granular, Compression Molded
Röchling Glastic BMC 1401 GTP Glass-Reinforced Polyester
A. Schulman BMC A50-XHS-U Bulk molding compound

PHAY00 / 45606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.