MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc  (discontinued **)
Categories: Polymer; Thermoplastic; Ionomer; Ionomer, Molded

Material Notes: Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutralization levels for this grade result in a combination of toughness, tear resistance, and clarity. The resin can be injection molded or extruded into sheets or shapes. It complies with the provisions of U.S. Food and Drug Administration (FDA) Title 21 Code of Regulations 177:1330 - ionomer resins.

Data provided by the manufacturer.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Key Words: Ethylene/Methacrylic Acid (E/MAA) Copolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792
Melt Flow 1.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
condition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ASTM D2240
Tensile Strength, Ultimate 28.3 MPaASTM D638
Tensile Strength, Yield 11.0 MPa50 mm/min cross speed; ASTM D638
Elongation at Break 460 %ASTM D638
Flexural Modulus 0.210 GPaASTM D790
Izod Impact, Notched NBASTM D256
Tensile Impact Strength 1240 kJ/m²ASTM D1822S
Abrasion 360NBS Index; ASTM D1630
 
Thermal PropertiesOriginal ValueComments
CTE, linear 160 µm/m-°C
@Temperature -20.0 - 32.0 °C
ASTM D696
Thermal Conductivity 0.250 W/m-K
Melting Point 90.0 °CDTA
Deflection Temperature at 0.46 MPa (66 psi) 40.0 °CASTM D648
Vicat Softening Point 73.0 °CRate B, ASTM D1525-70
Brittleness Temperature -100 °CASTM D746
Flame Spread 20.3 mm/minASTM D635
 
Optical PropertiesOriginal ValueComments
Haze 15 %
@Thickness 6.40 mm
ASTM D1003A
Gloss 25 %20° per ASTM D523-6

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Surlyn® 8920 Ionomer Resin, Sodium
Dow Surlyn® 9120 Ionomer Resin, Zinc
Dow Surlyn® 8150 Ionomer Resin, Sodium
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium
Dow Surlyn® 8020 Ionomer Resin, Sodium

PDU420 / 33071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.