MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 9392AU Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Extrusion- and injection molding grade; with special UV stabilizers; very good hydrolysis and microbial resistance; good low-temperature flexibility; Application; Hoses, non-reinforced; Cable sheathings; Profiles; Technical parts

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9292ISO 868
Hardness, Shore D 4242ISO 868
Tensile Strength, Ultimate 49.3 MPa7150 psi200 mm/min; DIN 53504
Tensile Stress at Strain  4.00 MPa
@Strain 10 %
580 psi
@Strain 10 %
200 mm/min; DIN 53504
 8.60 MPa
@Strain 50 %
1250 psi
@Strain 50 %
200 mm/min; DIN 53504
 10.8 MPa
@Strain 100 %
1570 psi
@Strain 100 %
200 mm/min; DIN 53504
 24.9 MPa
@Strain 300 %
3610 psi
@Strain 300 %
200 mm/min; DIN 53504
Elongation at Break 473 %473 %200 mm/min; DIN 53504
Tensile Modulus  0.0710 GPa
@Temperature 60.0 °C
10.3 ksi
@Temperature 140 °F
storage; ISO 3421-1,-4
 0.132 GPa
@Temperature 20.0 °C
19.1 ksi
@Temperature 68.0 °F
storage; ISO 3421-1,-4
 0.700 GPa
@Temperature -20.0 °C
102 ksi
@Temperature -4.00 °F
storage; ISO 3421-1,-4
Rebound 32 %32 %Resilience; ISO 4662
Tear Strength 85.0 kN/m485 pli500 mm/min; ISO 34-1
Abrasion 2020mm³, Method A; ISO 4649
Compression Set  20 %
@Temperature 23.0 °C
20 %
@Temperature 73.4 °F
72 hr; ISO 815
 57 %
@Temperature 70.0 °C
57 %
@Temperature 158 °F
24 hr; ISO 815
 35 %
@Temperature 70.0 °C,
Time 86400 sec
35 %
@Temperature 158 °F,
Time 24.0 hour
Method C; ISO 815-1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 215 °C383 - 419 °FExtrusion
 210 - 230 °C410 - 446 °FInjection
Mold Temperature 20.0 - 40.0 °C68.0 - 104 °FInjection
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 2792A GMP TPU
Covestro Desmopan® 9395AU Polyurethane
Covestro Desmopan® 9650DU Polyurethane
Covestro Desmopan® 9386A Polyurethane
Covestro Desmopan® 9392A GMP TPU

PB09817 / 92657

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.