MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay ALKAMULS® PSTO 20 Surfactant  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Good emulsification characteristics, particularly in combination with high or low HLB surfactants to form W/O or O/W emulsions.

Chemical Name: ETHOXYLATED SORBITAN TRIOLEATE

CAS: 9005-70-3; 7732-18-5

Solubility: Water- Dispersible; Mineral Oil-Dispersible; Aromatic- Dispersible; Aliphatic- Dispersible

Available in: Asia Pacific, Europe, Latin America and North America

Applications: ALKAMULS® PSTO-20 is used in the following applications: emulsifier and co-emulsifier for petroleum oils, fats and waxes, lubricant in textile and leather processing, emulsifier for textile finishes and fiberglass lubricant and emulsifier/lubricant in metal working formulations.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 2.0[mg KOH/g]; RP-0007
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 149 °CCOC; ASTM D92
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 9.0RP-0138
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 4.8 - 5.2 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear LiquidRP-0064
CompositionActive1
HLB number11
Hydroxyl Number39-52 mg KOH/gRP-0245
Ionic ChargeNonionic
Saponification number80-95 mg KOH/gRP-0496

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay ALKAMULS® OR 40 Surfactant
Schmelzer Industries Pearlveil 110-7 Fiberglass Veil
Schmelzer Industries Pearlveil 110-30 Fiberglass Veil
Schmelzer Industries Curveil 220-15 Fiberglass Veil
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat

WRHOD050 / 137280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.