MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Materion Beryllium Copper Alloy 25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17200)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: as supplied

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: ASTM B-197, QQ-C-530, AMS 4725
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.36 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 620 - 800 MPa
Tensile Strength, Yield 510 - 730 MPa
Elongation at Break 3.0 - 25 %
Modulus of Elasticity 131 GPa
Machinability 20 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000910 - 0.0000115 ohm-cm15-19% IACS Conductivity
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
Thermal Conductivity 105 W/m-K
Melting Point 870 - 980 °C
Solidus 870 °C
Liquidus 980 °C
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.8 - 2.0 %
Co + Ni >= 0.20 %
Co + Ni + Fe <= 0.60 %
Copper, Cu 98 %as balance
Lead, Pb <= 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion Beryllium Copper Alloy M25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17300)
Chromium-Copper, UNS C17600, TF00 Temper rod, bar, wire, tubing, plate, forged products
Materion Beryllium Copper Alloy 3 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17510)
Materion Brush® 1916 Machinable Copper Nickel Alloy Wire, Temper HT (UNS C19160)
Materion Brush 1915™ Heat Treated Temper Wire, 0.050" - 0.375"

NBB616 / 15246

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.