Product Description: FL 00728CC is an excellent coextrusion partner in extrusion coating, blown and cast film. Good adhesion onto OPP in coextrusion. This grade offers excellent optical, low gel and a very low Seal Initiation Temperature in sealing applications. Processing Conditions: Excellent results are obtained in extrusion coating at 200°C (392°F) temperature range. Processing temperatures above 220°C (428°F) may cause resin degradation. FL 00728CC should be fed into the extruder after LDPE of a similar or higher melt index. Machines should always be purged with LDPE or a suitable cleaning compound before shutdown.Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications:- Adhesive Lamination
- Adhesive Layer onto OPP
- Cling Layer
- Coextrusion Coating
- Compounding
- Extrusion Coating
- Extrusion Lamination
- High Frequency Sealing
- Industrial Packaging
- Injection Molding
- Masterbatch Base Resin
- Surface Protection Film
- Thermal Lamination
Information provided by ExxonMobil |