MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Desmodur® BL 1100/1 Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Blocked aromatic polyisocyanate based on TDI. In combination with cycloaliphatic diamines such as Laromin® C 260 (BASF) to formulate highly flexible, one-component stoving coatings.

Properties / Applications: Desmodur® BL 1100/1 is combined with Laromin® C 260 to formulate stoving coatings, including those for application by dipping and curtain coating, and adhesive cements. Combinations of Desmodur® BL 1100/1 and Laromin® C 260 with plasticisers can also be used as solvent-free, high-build coatings. Optimum film properties are produced by combining Desmodur® BL 1100/1 and Laromin® C 260 in the ratio 100 : 10 (by wt.). The mixing ratio was determined empirically.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/ccDIN EN ISO 2811
Viscosity 33000 - 53000 cPDIN EN ISO 3219/A.3
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 150 °CDIN EN 22 719
 
Descriptive Properties
Color<150Hazen, DIN EN 1557
Content<0.2%Free NCO content, DIN EN ISO 11 909 mod.
 3%NCO content, blocked

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODUR® LU-D80 + MOCA Polyurethane, TDI-Ester
Covestro Desmodur® E 15 Polyurethane
Covestro Acclaim® 2200 Polyol
Covestro DESMODUR® 0363 + BAYTEC® XL 0328 + BAYTEC® 0354 + BAYTEC® 0340 73A Polyurethane, MDI PPG
Covestro Desmodur® 30BV30 + (Baytec® 20BV29 + Baytec® XL9611 + Baytec® XL B) 79A Polyurethane, MDI Ester

PCOVEST0326 / 202109

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.