MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Momentive Performance Materials RTV6702 One-Component,  Modified Alkoxy Adhesive Sealant, White
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature.

These sealants are standard curing paste consistency products which can be applied to horizontal, vertical and overhead surfaces. They have a long work life which allows for tooling of finished assemblies.

Mechanical, electrical, and thermal properties for specimen cured 7 days at 25°C and 50% relative humidity.

Key Performance Properties:

  • Primerless adhesion to many metals and plastics
  • Non-corrosive to most substrates
  • Low odor cure
  • One-component product - No mixing required
  • Retain elastomeric properties at temperatures of -60C (-75F) to 204C (400F) for long periods and to 260C (500F) for short periods Room temperature cure
  • Excellent electrical insulation properties
  • Excellent UV, chemical and weather resistance

Applications:

The cure properties of these adhesive sealants make them ideally suited for applications in confined spaces. These paste-consistency silicone sealants can be used in thickness up to 6mm (1/4 in.) for bonding and sealing, joining metals and plastics, and electrical insulation.

For applications requiring sealant thickness greater than 6mm (1/4 in.), GE Silicones one-component, addition cure or two component silicone rubber compounds are recommended.

GE Silicones became a part of Momentive Performance Materials in 2006.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1818
Tensile Strength, Ultimate 1.55 MPa225 psi
Elongation at Break 450 %450 %
Tear Strength 4.90 kN/m28.0 pli
Peel Strength 5.78 kN/m33.0 pliPVC
 6.14 kN/m35.0 pliGlass
 6.14 kN/m35.0 pliAluminum
 6.49 kN/m37.0 pliLexan Polycarbonate®
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cm
Dielectric Constant 2.9
@Frequency 100 Hz
2.9
@Frequency 100 Hz
Dielectric Strength 16.0 kV/mm406 kV/in
Dissipation Factor 0.00020
@Frequency 100 Hz
0.00020
@Frequency 100 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 300 µm/m-°C
@Temperature 20.0 °C
167 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°F
Brittleness Temperature -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourThrough
Tack-Free Time 25.0 min0.417 hour
 
Descriptive Properties
Application rate175 g/min
ColorWhite
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV658A Low Volatile Silicone Adhesive Sealant Component, White
Momentive Performance Materials RTV658 Low Volatile Silicone Adhesive Sealant, White, Mixed
Momentive Performance Materials RTV6703 One-Component,  Modified Alkoxy Adhesive Sealant, Black
Momentive Performance Materials RTV658B Low Volatile Silicone Adhesive Sealant Component, Clear
Permabond 940 Cyanoacrylate, low odor

PGESIL051 / 41042

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.