MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Dehesive® 915 Silicone Release Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: DEHESIVE® 915 is 100 %, completely solvent-free, addition-curing silicone intended for coating paper and other substrates.

Special features:

  • extremely fast curing
  • medium release at low peel speeds
  • low release at high peel speeds
  • flat release profile
  • good release stability
  • good bath life
  • solvent-free
  • good coverage at low silicone coat weights
  • extremely fast cure properties of DEHESIVE® 915 allow for a very low platinum concentration
Application: DEHESIVE® 915 is solvent-free silicones with an oily consistency and good flow properties. It is especially suitable for solvent-free paper coating. Other substrates can be rendered non-stick towards pressure-sensitive adhesives with this product, e.g. metallic tapes and plastic sheets. DEHESIVE® 915 develops optimum release properties once it has undergone complete crosslinking. Subsequent postcuring - which is needed for most condensation-crosslinking silicones - is not necessary.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccDIN 51757
Viscosity 120 cPdynamic
Storage Temperature 20.0 °C12 months
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 150 °CISO 2719
Ignition Temperature >= 350 °Cliquids; DIN 51794
 
Descriptive Properties
Active ingredients (%)100
Appearancecolorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Dehesive® 919 Silicone Release Coating
Wacker Dehesive® 944 Silicone Release Coating
Wacker Dehesive® SFX 251 AMA® Silicone Release Coating
Wacker Dehesive® SFX 250 Silicone Release Coating
Wacker Dehesive® SF 500 Silicone Release Coating

PWACK9066 / 204595

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.