MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Renishaw 420 Hand/Vacuum casting resin
Categories: Polymer; Thermoset

Material Notes: Description: Hand/vacuum casting resin-slow curing version of 410

Features: Outstanding mechanical properties

Suitable for: As 410, but for larger models, Can be highly filled for casting of very thick section moldings

Information provided by Renishaw

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccPart A
 1.08 g/cc1.08 g/ccPart B
Viscosity 80 cP80 cPPart A
 80 cP80 cPPart B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575Cured; ISO 868
Tensile Strength 30.0 MPa4350 psiCured; ISO R 527
Flexural Strength 40.0 MPa5800 psiCured; ISO 178
Flexural Modulus 1.02 GPa148 ksiCured; ISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C154 °FCured, (test piece 110 mm × 12.7 mm × 6.4 mm); ISO 75
Glass Transition Temp, Tg 80.0 °C176 °FCured
Shrinkage 0.50 - 1.0 %0.50 - 1.0 %
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 40.0 °C68.0 - 104 °FResin Temp
Mold Temperature 30.0 - 70.0 °C86.0 - 158 °F
Cure Time 35.0 - 80.0 min
@Temperature 30.0 - 70.0 °C
0.583 - 1.33 hour
@Temperature 86.0 - 158 °F
Pot Life 5.00 min
@Load 0.100 kg
5.00 min
@Load 0.221 lb
 
Descriptive Properties
ColorWhite
Mixing ratio by weightA:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 420 Martensitic Stainless steel
Kinetics MIM 420 Stainless Steel (Oil Quench Heat Treat)
Renishaw 6230 Vacuum casting resin
Renishaw 3176 Vacuum casting resin
Latrobe LSS™ 420 HC High Carbon Stainless Steel

PRENISH018 / 206381

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.