MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Palladium, Pd
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy; Pure Element

Material Notes: Physical Form: Silver-White Metal; Cubic

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 12.02 g/cc0.4343 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 106.42106.421995
Atomic Number 4646
Thermal Neutron Cross Section 8.0 barns/atom8.0 barns/atom
X-ray Absorption Edge 0.509 Å0.509 ÅK
 3.42999 Å3.42999 ÅLI
 3.7136 Å3.7136 ÅLII
 3.89688 Å3.89688 ÅLIII
Electrode Potential -0.570 V-0.570 V
Electronegativity 2.22.2Pauling
Ionic Radius 0.650 Å0.650 ÅCrystal Ionic Radius for Valence +4
 0.800 Å0.800 ÅCrystal Ionic Radius for Valence +2
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 3737Annealed
 105105Cold Drawn
Tensile Strength, Ultimate 180 MPa26100 psiAnnealed
 320 MPa46400 psiCold Drawn
Elongation at Break 2.0 %2.0 %Cold Drawn
 30 - 40 %30 - 40 %Annealed
Modulus of Elasticity 117 GPa17000 ksi
Poissons Ratio 0.390.39
Shear Modulus 42.0 GPa6090 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000993 ohm-cm0.00000993 ohm-cm
Magnetic Susceptibility 0.00000580.0000058cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 17.6 J/g7.57 BTU/lb
Heat of Vaporization 373 J/g160 BTU/lb
CTE, linear  11.1 µm/m-°C
@Temperature 20.0 - 100 °C
6.17 µin/in-°F
@Temperature 68.0 - 212 °F
 12.2 µm/m-°C
@Temperature 0.000 - 250 °C
6.78 µin/in-°F
@Temperature 32.0 - 482 °F
 12.8 µm/m-°C
@Temperature 0.000 - 500 °C
7.11 µin/in-°F
@Temperature 32.0 - 932 °F
 13.9 µm/m-°C
@Temperature 0.000 - 1000 °C
7.72 µin/in-°F
@Temperature 32.0 - 1830 °F
Specific Heat Capacity 0.195 J/g-°C0.0466 BTU/lb-°FGas
 0.247 J/g-°C0.0590 BTU/lb-°F
Thermal Conductivity 71.2 W/m-K494 BTU-in/hr-ft²-°F
Melting Point 1552 °C2826 °F
Boiling Point 2963 °C5365 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 378.2 kJ/mol378.2 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.330.3365 micron
Reflection Coefficient, Visible (0-1) 0.6280.628white light
 
Component Elements PropertiesMetricEnglishComments
Palladium, Pd 100 %100 %
 
Descriptive Properties
SolubilitySoluble in Aqua Regia

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gold, Au
Silver, Ag
Aluminum, Al
Nickel, Ni
Platinum, Pt, CP Grade, Annealed

AMEPd00 / 81

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.