System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 30% Glass Fiber Filled
Material Notes:
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.
Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America
Information provided by Lati Industria Termoplastici S.p.A.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.30
g/cc
Linear Mold Shrinkage, Flow
0.0045
-
0.0075
cm/cm
Linear Mold Shrinkage, Transverse
0.0090
-
0.012
cm/cm
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
45.0
MPa
@Temperature 150 °C
55.0
MPa
@Temperature 120 °C
65.0
MPa
@Temperature 90.0 °C
85.0
MPa
@Temperature 60.0 °C
120
MPa
@Temperature 23.0 °C
Elongation at Break
3.5 %
@Temperature 23.0 °C
5.0 %
@Temperature 60.0 °C
6.0 %
@Temperature 90.0 °C
6.5 %
@Temperature 120 °C
6.5 %
@Temperature 150 °C
Elongation at Yield
4.0 %
@Temperature 60.0 °C
5.5 %
@Temperature 90.0 °C
6.0 %
@Temperature 120 °C
6.0 %
@Temperature 150 °C
Tensile Modulus
410
MPa
@Temperature 90.0 °C
2800
MPa
@Temperature 150 °C
3100
MPa
@Temperature 120 °C
5700
MPa
@Temperature 60.0 °C
8000
MPa
@Temperature 23.0 °C
Charpy Impact Unnotched
65.0
kJ/m²
@Temperature 23.0 °C
75.0
kJ/m²
@Temperature -20.0 °C
Charpy Impact, Notched
10.0
kJ/m²
@Temperature -20.0 °C
15.0
kJ/m²
@Temperature 23.0 °C
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
100
°C
Deflection Temperature at 0.46 MPa (66 psi)
260
°C
Deflection Temperature at 1.8 MPa (264 psi)
240
°C
Vicat Softening Point
245
°C
@Load 5.00 kg
Processing Properties
Original Value
Comments
Melt Temperature
260
-
290
°C
Mold Temperature
60.0
-
80.0
°C
Drying Temperature
90.0
-
100
°C
@Time 10800 sec
Descriptive Properties
ISO Shrinkage - Pressure
60 MPa
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Domo TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY
Envalior Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber
Envalior Durethan® DP AKV 35 LT H2.0 904040 Nylon 66, 35% Glass Fiber
Avient Edgetek® NN-35MG/000 Black v1.1 Polyamide 66 (Nylon 66)
Celanese Zytel® 70G35EF BK538 PA66-GF35
PLATH9704 / 177400
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.