MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
LyondellBasell Pro-fax 7531 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Primary Processing Method: Injection Molding/Thermoforming

Key Features: medium impact polypropylene copolymer resin for food packaging, FDA acceptable, low odor and low taste transfer, good cold impact resistance, excellent dimensional stability

Applications: food containers, medical wares, housewares

Meets FDA requirements in 21 CFR 177.1520 for all food contact, including cooking applications.

Description: Pro-fax 7531 medium impact polypropylene copolymer resin is designed for food packaging applications. It can be used on standard injection molding and thermoforming equipment. It has passed USP Class VI testing. It has a yellow card RTI, which applies to all colors. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792B
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 27.0 MPaASTM D638
Elongation at Yield 8.0 %ASTM D638
Flexural Modulus, 1% Secant 1.20 GPa0.05 in/min; ASTM D790A
Izod Impact, Notched 1.10 J/cmASTM D256A
Impact Test 26.0 J
@Temperature -29.0 °C
Montell drop weight impact strength
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CASTM D648
UL RTI, Mechanical with Impact 65.0 °C
@Thickness >=0.991 mm
Flammability, UL94 HB
@Thickness >=0.991 mm
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer
LyondellBasell Montell SE191 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHM-200 Polypropylene Impact Copolymer
Chevron Phillips Marlex® AHN-230 Polypropylene Impact Copolymer

PMO183 / 53550

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.